China wholesale Welding Procedure Data Sheet Factory - AWS E7015-B2L Low-alloy steels Manual electrode Welding jointing – Honest Metal
China wholesale Welding Procedure Data Sheet Factory - AWS E7015-B2L Low-alloy steels Manual electrode Welding jointing – Honest Metal Detail:
Application&Standard&Note:
AWS E7015-B2L heat resistant steel electrode is suitable for welding boiler heating surface tube and power plant water wall, steam pipe and high pressure vessel working temperature below 550℃, such as 15CrMo tube plate, A335-P11 tube, A387Gr.11 plate. And can be used for 30CrMnSi casting welding, suitable for the occasion of low carbon content requirements. In addition, it is necessary to preheat the weldment at the inter-channel temperature of 160℃~190℃ during welding, and 690±15℃*1h heat treatment should be carried out according to the standard requirements of welding materials.
Features
AWS E7015-G2L(R307L) type heat-resistant steel hand electrode is a low sodium hydrogen type hand electrode, stable arc, less splash, good forming, easy desagging, X-Ray performance is excellent. It has stable mechanical properties and can maintain high impact toughness under heat treatment conditions. Preheating is an important technological measure for welding cold cracks and eliminating stress of perlite heat resistant steel. In order to ensure the quality of welding, no matter in the process of spot solid welding or welding, it should be preheated and maintain a certain temperature range. After the end of the welding work to welding slow cooling, welding slow cooling is the welding chromium-molybdenum heat resistant steel must strictly follow the principle, even in the hot summer must do this, general welding immediately with asbestos cloth to cover the weld and near the seam area, small welding parts can be placed in the asbestos cloth slow cooling.
Company & Factory
Product composition and mechanical properties introduction
CHEMICAL COMPONET:
ALLOY(wt%) | C | Mn | Si | Cr | Mo | P | S | Ni |
GB/T RULES | 0.05 | 0.90 | 1.00 | 1.00-1.50 | 0.40-0.65 | 0.03 | 0.030 | - |
AWS RULES | 0.05 | 0.90 | 1.00 | 1.00-1.50 | 0.40-0.65 | 0.04 | 0.035 | - |
EXAMPLE VALUE | 0.038 | 0.85 | 0.26 | 1.2 | 0.48 | 0.013 | 0.009 | 0.020 |
MECHANICAL PROPERTY:
PROPERTY | YIELD STRENGTH(MPa) | EXTENSION STRENGTH(MPa) | HEATTREAMENT℃xh | IMAPACT VALUE J/℃ | ELONGATION(%) | |||||||||
GB/T RULES | 390 | 520 | 690*1 | - | 17 | |||||||||
AWS RULES | 390 | 520 | 690*1 | - | 19 | |||||||||
EXAMPLE VALUE | 450 | 550 | 690*1 | 185/Nature temperature | 28 |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | ||||||
ELECTRICITY (Amp) |
H/W | 80-110 | 100-130 | 130-180 | 170-210 | |||||
O/W | 60-100 | 80-120 | 120-160 | - |
PACKING DETAILES:
SEPCIFICATION | LENGTH | PCS/1KG | WEIGHT/1KG | |||
2.6mm | 300mm | 48PCS | 2KG | |||
3.2mm | 350mm | 27PCS | 5KG | |||
4.0mm | 350mm | 16PCS | 5KG | |||
5.0mm | 350mm | 12PCS | 5KG |
Typical Cases
Certificate
Product detail pictures:




Related Product Guide:
We know that we only thrive if we will guarantee our combined cost competiveness and high-quality advantageous at the same time for China wholesale Welding Procedure Data Sheet Factory - AWS E7015-B2L Low-alloy steels Manual electrode Welding jointing – Honest Metal , The product will supply to all over the world, such as: Seychelles, Portugal, Plymouth, Our company is an international supplier on this kind of merchandise. We offer an amazing selection of high-quality products. Our goal is to delight you with our distinctive collection of mindful products while providing value and excellent service. Our mission is simple: To provide the best products and service to our customers at the lowest prices possible.

The enterprise has a strong capital and competitive power, product is sufficient, reliable, so we have no worries on cooperating with them.