Application&Standard&Note:
AWS E7015-B2L heat resistant steel electrode is suitable for welding boiler heating surface tube and power plant water wall, steam pipe and high pressure vessel working temperature below 550℃, such as 15CrMo tube plate, A335-P11 tube, A387Gr.11 plate. And can be used for 30CrMnSi casting welding, suitable for the occasion of low carbon content requirements. In addition, it is necessary to preheat the weldment at the inter-channel temperature of 160℃~190℃ during welding, and 690±15℃*1h heat treatment should be carried out according to the standard requirements of welding materials.
Features
AWS E7015-G2L(R307L) type heat-resistant steel hand electrode is a low sodium hydrogen type hand electrode, stable arc, less splash, good forming, easy desagging, X-Ray performance is excellent. It has stable mechanical properties and can maintain high impact toughness under heat treatment conditions. Preheating is an important technological measure for welding cold cracks and eliminating stress of perlite heat resistant steel. In order to ensure the quality of welding, no matter in the process of spot solid welding or welding, it should be preheated and maintain a certain temperature range. After the end of the welding work to welding slow cooling, welding slow cooling is the welding chromium-molybdenum heat resistant steel must strictly follow the principle, even in the hot summer must do this, general welding immediately with asbestos cloth to cover the weld and near the seam area, small welding parts can be placed in the asbestos cloth slow cooling.
Company & Factory
Product composition and mechanical properties introduction
CHEMICAL COMPONET:
ALLOY(wt%) | C | Mn | Si | Cr | Mo | P | S | Ni |
GB/T RULES | 0.05 | 0.90 | 1.00 | 1.00-1.50 | 0.40-0.65 | 0.03 | 0.030 | - |
AWS RULES | 0.05 | 0.90 | 1.00 | 1.00-1.50 | 0.40-0.65 | 0.04 | 0.035 | - |
EXAMPLE VALUE | 0.038 | 0.85 | 0.26 | 1.2 | 0.48 | 0.013 | 0.009 | 0.020 |
MECHANICAL PROPERTY:
PROPERTY | YIELD STRENGTH(MPa) | EXTENSION STRENGTH(MPa) | HEATTREAMENT℃xh | IMAPACT VALUE J/℃ | ELONGATION(%) | |||||||||
GB/T RULES | 390 | 520 | 690*1 | - | 17 | |||||||||
AWS RULES | 390 | 520 | 690*1 | - | 19 | |||||||||
EXAMPLE VALUE | 450 | 550 | 690*1 | 185/Nature temperature | 28 |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | ||||||
ELECTRICITY (Amp) |
H/W | 80-110 | 100-130 | 130-180 | 170-210 | |||||
O/W | 60-100 | 80-120 | 120-160 | - |
PACKING DETAILES:
SEPCIFICATION | LENGTH | PCS/1KG | WEIGHT/1KG | |||
2.6mm | 300mm | 48PCS | 2KG | |||
3.2mm | 350mm | 27PCS | 5KG | |||
4.0mm | 350mm | 16PCS | 5KG | |||
5.0mm | 350mm | 12PCS | 5KG |
Typical Cases
Certificate
Product detail pictures:




Related Product Guide:
Our company since its inception, always regards product quality as enterprise life, continuously improve production technology, improve product quality and continuously strengthen enterprise total quality management, in strict accordance with the national standard ISO 9001:2000 for China wholesale Welding Procedure Data Sheet Manufacturers - AWS E7015-B2L Low-alloy steels Manual electrode Welding jointing – Honest Metal , The product will supply to all over the world, such as: Honduras, Kyrgyzstan, Auckland, Our organization. Situated inside the national civilized cities, the visitors is very easy, unique geographical and economic situations. We pursue a people-oriented, meticulous manufacturing, brainstorm, construct brilliant organization. hilosophy. Strict top quality management, fantastic service, reasonable cost in Myanmar is our stand on the premise of competition. If vital, welcome to make contact with us by our web page or telephone consultation, we are going to be pleased to serve you.

Perfect services, quality products and competitive prices, we have work many times, every time is delighted, wish continue to maintain!