China wholesale Welding Procedure Data Sheet Manufacturers - AWS E8015-B3L Low-alloy steels Metal powder welding wire Welding connection – Honest Metal
China wholesale Welding Procedure Data Sheet Manufacturers - AWS E8015-B3L Low-alloy steels Metal powder welding wire Welding connection – Honest Metal Detail:
Application&Standard&Note:
AWS E8015-B3L type heat-resistant steel hand electrode equivalent to GB/T 5118 standard electrode model E5515-2C1ML electrode, in line with ISO 3580-B standard electrode model E5515-2CIML, is a suitable for 550℃ under high temperature and high pressure pipeline, synthetic chemical machinery, Petroleum cracking equipment, such as 2.5Cr1Mo tube plate, A335-P22 tube, A387Gr.22 plate. We strictly control the supply of raw materials, through advanced production technology processing production, each batch of goods are finished product inspection, to customers have a perfect after-sales service. We pay attention to every detail of the process. Only to provide higher quality products.
Features
AWS E8015-B3L type hand welding electrode for heat resistant steel is a low sodium hydrogen type hand welding electrode, which still has excellent creep resistance under 550℃ high temperature and high pressure working conditions, and the electrode has stable arc, less splashing, good forming, easy de-slagging and excellent X-Ray performance. When welding, thick plate should be multi-layer welding, the temperature between the layers is not lower than the preheating temperature, welding should be finished at a time, it is better not to interrupt. If interlayer pause is needed, thermal insulation and slow cooling measures should be taken, and the same preheating measures should be taken before rewelding. During the welding process, attention should be paid to filling the arc pit, grinding the joint, and removing the arc pit crack (hot crack). The larger the current is, the deeper the arc pit is. Therefore, the welding parameters and the appropriate welding line energy should be selected in strict accordance with the welding process instructions.
Company & Factory
Product composition and mechanical properties introduction
CHEMICAL COMPONET:
ALLOY(wt%) | C | Mn | Si | Cr | Mo | P | S | Ni |
GB/T RULES | 0.05 | 0.90 | 1.00 | 2.00–2.50 | 0.90-1.20 | 0.03 | 0.030 | - |
AWS RULES | 0.05 | 0.90 | 1.00 | 2.00–2.50 | 0.90-1.20 | 0.03 | 0.030 | - |
EXAMPLE VALUE | 0.045 | 0.66 | 0.31 | 2.25 | 1.05 | 0.013 | 0.007 | 0.023 |
MECHANICAL PROPERTY:
PROPERTY | YIELD STRENGTH(MPa) | EXTENSION STRENGTH(MPa) | HEATTREAMENT℃xh | IMAPACT VALUE J/℃ | ELONGATION(%) | |||||||||
GB/T RULES | 460 | 550 | 690*1 | - | 15 | |||||||||
AWS RULES | 460 | 550 | 690*1 | - | 17 | |||||||||
EXAMPLE VALUE | 500 | 600 | 690*1 | 170/Nature temperature | 21 |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | ||||||
ELECTRICITY (Amp) |
H/W | 80-110 | 100-130 | 130-180 | 170-210 | |||||
O/W | 60-100 | 80-120 | 120-160 | - |
PACKING DETAILES:
SEPCIFICATION | LENGTH | PCS/1KG | WEIGHT/1KG | |||
2.6mm | 300mm | 48PCS | 2KG | |||
3.2mm | 350mm | 27PCS | 5KG | |||
4.0mm | 350mm | 16PCS | 5KG | |||
5.0mm | 350mm | 12PCS | 5KG |
NOTE:
H/W: horizontal position welding
O/W: over-head position welding
Typical Cases
Certificate
Product detail pictures:




Related Product Guide:
In order to best meet client's needs, all of our operations are strictly performed in line with our motto High Quality, Competitive Price, Fast Service for China wholesale Welding Procedure Data Sheet Manufacturers - AWS E8015-B3L Low-alloy steels Metal powder welding wire Welding connection – Honest Metal , The product will supply to all over the world, such as: California, Romania, Algeria, Good quality, Good service is always our tenet and credo. We take every effort to control the quality, package, labels etc and our QC will check every detail during producing and before shipment. We have been willing to establish long business relationship with all those who seek the high quality products and good service. We've got set up a wide sales network across European countries, North of America, South of America, Middle East, Africa, East Asia countries.Please contact us now, you will find our expert experience and high quality grades will contribute to your business.

The product classification is very detailed that can be very accurate to meet our demand, a professional wholesaler.