CHEMICAL COMPONET:
ALLOY(wt%) | C | Mn | Si | Ni | Cr | Mo | P | S |
GB/T RULES | 0.12 | 1.25 | 0.80 | 3.00-3.75 | - | - | 0.03 | 0.03 |
AWS RULES | 0.12 | 1.25 | 0.80 | 3.00-3.75 | - | - | 0.03 | 0.03 |
EXAMPLE VALUE | 0.045 | 0.75 | 0.22 | 3.52 | 0.04 | 0.06 | 0.007 | 0.004 |
MECHANICAL PROPERTY:
PROPERTY | YIELD STRENGTH(MPa) | EXTENSION STRENGTH(MPa) | IMAPACT VALUE J/℃ | ELONGATION(%) | Heat treatment°Cxh | |||||
GB/T RULES | 460 | 550 | 27/-75 | 17 | 605*1 | |||||
AWS RULES | 460 | 550 | 27/-75 | 19 | 605*1 | |||||
EXAMPLE VALUE | 495 | 600 | 100/-75 | 26 | 605*1 |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | ||||
ELECTRICITY (Amp) |
H/W | 80-110 | 100-130 | 130-180 | 170-210 | |||
O/W | 60-100 | 80-120 | 120-160 | - |
Speciality
Iron powder low hydrogen type hand electrode.
Due to the addition of iron powder, the melting efficiency is higher, the impact toughness of the molten metal at -75℃.
Stable arc, less splash, good forming, easy slag removal, X-Ray performance is excellent.
Show detail
Shipment
About us
Actual factory shooting
Applaication case
Product detail pictures:




Related Product Guide:
We stay with the basic principle of quality initially, services first, steady improvement and innovation to fulfill the customers for your management and zero defect, zero complaints as the quality objective. To perfect our company, we give the goods while using the good high-quality at the reasonable selling price for China wholesale Welding Procedure Data Sheet Suppliers - Low-alloy steels Manual electrode E8018-C2 Soldering data – Honest Metal , The product will supply to all over the world, such as: California, Victoria, Leicester, Each product is carefully made, it will make you satisfied. Our merchandise in the production process have got strictly monitored, because it is only to supply you the best quality, we'll feel confident. High production costs but low prices for our long-term cooperation. You can have a variety choices and the value of all types are same reliable. If you have any question, do not hesitate to ask us.

After the signing of the contract, we received satisfactory goods in a short term, this is a commendable manufacturer.

Write your message here and send it to us