High Carbon Steels Manual Electrode E11018M jack-up rigs Consumables
Suitable for low alloy steel welding of the same strength grade in construction machinery, such as Q690, etc.
The standard we met: GB/T32533 E7618-N4M2, AWS A5.5 E11018M & A5.5M E7618M, ISO18275-A:E 69 5 Z1.5Mn2NiMo B 3 2, ISO 18275-B: E7618-N4M2 A JIS Z 3211 E 7618-N4M2L.
What are the
characieristics?
●Iron powder low hydrogen potassium hand electrode, high efficiency.
●Stable arc, small splash, good molding.
●Easy desagging, X-ray performance is good.
●Stable mechanical properties.
Product Parameter
CHEMICAL COMPONET:
ALLOY(wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | V |
GB/T RULES | 0.10 | 1.30-1.80 | 0.60 | 0.40 | 1.25-2.50 | 0.25-0.50 | 0.030 | 0.030 | 0.05 |
AWS RULES | 0.10 | 1.30-1.80 | 0.60 | 0.40 | 1.25-2.50 | 0.25-0.50 | 0.030 | 0.030 | 0.05 |
EXAMPLE VALUE | 0.067 | 1.69 | 0.3 | 0.13 | 2.29 | 0.38 | 0.007 | 0.004 | 0.007 |
MECHANICAL PROPERTY:
PROPERTY | YIELD STRENGTH(MPa) | EXTENSION STRENGTH(MPa) | HEATTREAMENT℃xh | IMAPACT VALUE J/℃ | ELONGATION(%) | ||||
GB/T RULES | 680-760 | 760 | AW | 27/-50 | 18 | ||||
AWS RULES | 400 | 490 | AW | 27/-50 | 20 | ||||
EXAMPLE VALUE | 415 | 570 | AW | 80/-50 | 22 |
RECOM MEN DED WEL .DING PARAMETERS :
DIAMETERS SPECIFICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | |||||
ELECTRICITY (Amp) |
H/W | 80-110 | 100-130 | 130-180 | 180-230 | ||||
O/W | 50-80 | 90-120 | 130-160 | - |
Look at the way
we transport
●Motor transport
●Shipping
Look at
our warenouse
●Sino-science Refining and Chemical 20 million tons/year refining and chemical integration project
Our products
to the world
CHEMICAL COMPONET:
ALLOY(wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | V |
GB/T RULES | 0.10 | 1.30-1.80 | 0.60 | 0.40 | 1.25-2.50 | 0.25-0.50 | 0.030 | 0.030 | 0.05 |
AWS RULES | 0.10 | 1.30-1.80 | 0.60 | 0.40 | 1.25-2.50 | 0.25-0.50 | 0.030 | 0.030 | 0.05 |
EXAMPLE VALUE | 0.067 | 1.69 | 0.3 | 0.13 | 2.29 | 0.38 | 0.007 | 0.004 | 0.007 |
MECHANICAL PROPERTY:
PROPERTY | YIELD STRENGTH(MPa) | EXTENSION STRENGTH(MPa) | HEATTREAMENT℃xh | IMAPACT VALUE J/℃ | ELONGATION(%) | ||||
GB/T RULES | 680-760 | 760 | AW | 27/-50 | 18 | ||||
AWS RULES | 400 | 490 | AW | 27/-50 | 20 | ||||
EXAMPLE VALUE | 415 | 570 | AW | 80/-50 | 22 |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | |||||
ELECTRICITY (Amp) |
H/W | 80-110 | 100-130 | 130-180 | 180-230 | ||||
O/W | 50-80 | 90-120 | 130-160 | - |