Low-alloy steels Manual electrode E7015-C1L Soldering jointing
CHEMICAL COMPONET:
ALLOY(wt%) | C | Mn | Si | Cr | Ni | Mo | P | S |
GB/T RULES | 0.12 | 1.25 | 0.60 | - | 2.0-2.75 | - | 0.03 | 0.03 |
AWS RULES | 0.05 | 1.25 | 0.50 | - | 2.0-2.75 | - | 0.03 | 0.03 |
EXAMPLE VALUE | 0.04 | 0.65 | 0.2 | 0.018 | 2.56 | 0.06 | 0.007 | 0.006 |
MECHANICAL PROPERTY:
PROPERTY | YIELD STRENGTH(MPa) | EXTENSION STRENGTH(MPa) | IMAPACT VALUE J/℃ | ELONGATION(%) | Heat treatment°Cxh | |||||
GB/T RULES | 390 | 490 | 27/-75 | 20 | 605*1 | |||||
AWS RULES | 390 | 490 | 27/-75 | 22 | 605*1 | |||||
EXAMPLE VALUE | 410 | 520 | 105/-75 | 26 | 605*1 |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | ||||
ELECTRICITY (Amp) |
H/W | 80-110 | 100-130 | 130-180 | 170-210 | |||
O/W | 60-100 | 80-120 | 120-160 | - |
The main composition is 2.5%Ni steel.
Low hydrogen potassium drug skin, the metal cladding at -75°C has excellent impact toughness.
Stable arc, less splash, good forming, easy slag removal, X-Ray performance is excellent.
180,000 tons Capesize bulk carrier
Shanghai Morimatsu Storage tank
Polypropylene reactor
CHEMICAL COMPONET:
ALLOY(wt%) | C | Mn | Si | Cr | Ni | Mo | P | S |
GB/T RULES | 0.12 | 1.25 | 0.60 | - | 2.0-2.75 | - | 0.03 | 0.03 |
AWS RULES | 0.05 | 1.25 | 0.50 | - | 2.0-2.75 | - | 0.03 | 0.03 |
EXAMPLE VALUE | 0.04 | 0.65 | 0.2 | 0.018 | 2.56 | 0.06 | 0.007 | 0.006 |
MECHANICAL PROPERTY:
PROPERTY | YIELD STRENGTH(MPa) | EXTENSION STRENGTH(MPa) | IMAPACT VALUE J/℃ | ELONGATION(%) | Heat treatment°Cxh | |||||
GB/T RULES | 390 | 490 | 27/-75 | 20 | 605*1 | |||||
AWS RULES | 390 | 490 | 27/-75 | 22 | 605*1 | |||||
EXAMPLE VALUE | 410 | 520 | 105/-75 | 26 | 605*1 |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | ||||
ELECTRICITY (Amp) |
H/W | 80-110 | 100-130 | 130-180 | 170-210 | |||
O/W | 60-100 | 80-120 | 120-160 | - |