Low-alloy steels Manual electrode E8018-B1 metal Jointing accessories
Iron powder low hydrogen potassium type hand electrode
Stable arc, less splash, good molding, easy slag removal.
X-Ray performance is excellent.
CHEMICAL COMPONET:
ALLOY(wt%) | C | Si | Mn | P | S | Ni | Cr | Mo | Other |
GB/T RULES | 0.075 | 0.33 | 0.78 | 0.013 | 0.009 | 0.015 | 0.55 | 0.53 | - |
MECHANICAL PROPERTY:
PROPERTY | YIELD STRENGTH(MPa) | EXTENSION STRENGTH(MPa) | Elongation(%) | IMAPACT VALUE J/℃ | Heat treatment °C*h | |||||
GB/T RULES | 520 | 620 | 25 | 130/Normal temperature | 620*1 |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 3.2*350 | 4.0*400 | 5.0*400 | ||||
ELECTRICITY (Amp) |
H/W | 90-130 | 140-190 | 190-240 | |||
O/W | 80-120 | 120-160 | - |
-
10000TEU container ship
SG superior nucleus
Wind power application
CHEMICAL COMPONET:
ALLOY(wt%) | C | Si | Mn | P | S | Ni | Cr | Mo | Other |
GB/T RULES | 0.075 | 0.33 | 0.78 | 0.013 | 0.009 | 0.015 | 0.55 | 0.53 | - |
MECHANICAL PROPERTY:
PROPERTY | YIELD STRENGTH(MPa) | EXTENSION STRENGTH(MPa) | Elongation(%) | IMAPACT VALUE J/℃ | Heat treatment °C*h | |||||
GB/T RULES | 520 | 620 | 25 | 130/Normal temperature | 620*1 |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 3.2*350 | 4.0*400 | 5.0*400 | ||||
ELECTRICITY (Amp) |
H/W | 90-130 | 140-190 | 190-240 | |||
O/W | 80-120 | 120-160 | - |