Low-alloy steels Manual electrode E9015-B91 Welding data

GB/T5118 E6215-9C1MV

AWS A5.5 E9015-B91

A5.5M E6215-B91

ISO 3580-A:E(CrMo91)B 4 2

ISO 3580-B:E6215-9C1MV

Whatapp:+8613252436578

E-mail: sale@welding-honest.com


  • Brand: JINGLEI
  • Model: GER-91(R717)
  • Power supply polarity: DC+
  • Origin: China
  • Suit for: Low-alloy steels
  • Size: 2.6*350mm 3.2*350mm 4.0*400mm 5.0*400mm
  • MOQ:1T Capacity: 1200T Per month
  • Payment: TT,LC
  • OEM: Can customerized
  • Product Detail

    SPECIFICATION

    Product Tags

    未标题-1
    fd1
    未标题-2

    CHEMICAL COMPONET:

    ALLOY(wt%) C Mn Si Cr Mo Ni P S V Cu AI Nb N
    GB/T RULES 0.08-0.13 1.25 0.30 8-10.5 0.85-1.2 1.00 0.01 0.01 0.15-0.30 0.25 0.04 0.02-0.10 0.02-0.07
    AWS RULES 0.08-0.13 1.20 0.30 8-10.5 0.85-1.2 0.80 0.01 0.01 0.15-0.30 0.25 0.04 0.02-0.10 0.02-0.07
    EXAMPLE VALUE 0.092 0.7 0.24 9 9 0.48 0.008 0.006 0.2 0.02 0.001 0.04 0.03

     

    MECHANICAL PROPERTY:

    PROPERTY YIELD STRENGTH(MPa) EXTENSION STRENGTH(MPa) IMAPACT VALUE J/℃ ELONGATION(%) Heat treatment°Cxh
    GB/T RULES 530 620 - 15 760*2
    AWS RULES 530 620 - 17 760*2
    EXAMPLE VALUE 585 730 78/Normal temperature 20 760*2

     

    RECOMMENDED WELDING PARAMETERS:

    DIAMETERS SPECIFICATIONS(mm) 2.6*350 3.2*350 4.0*400 5.0*400
    ELECTRICITY
    (Amp)
    H/W 80-110 100-130 130-180 170-210
    O/W 60-100 80-120 120-160 -

    Speciality

    01

    Low sodium hydrogen type hand electrode, core wire transition type.

    Add a small amount of Nb, V, used at 550 to 650 core temperature can have excellent creep resistance.

    02
    03

    Stable arc, less splash, good forming, easy slag removal, X-Ray performance is excellent.

    Show detail

    04
    05

    Shipment

    06
    07

    About us

    b0780de687c3deca16d616279ad5fd6

    Actual factory shooting

    08
    09
    10
    11

    Applaication case

    12
    13
    14
    • 37,000 tons general cargo ship

    • Safety injection box

    • Xinjiang Kela 2 Central treatment plant project

    Actual factory shooting

    577445SDA01

    CHEMICAL COMPONET:

    ALLOY(wt%) C Mn Si Cr Mo Ni P S V Cu AI Nb N
    GB/T RULES 0.08-0.13 1.25 0.30 8-10.5 0.85-1.2 1.00 0.01 0.01 0.15-0.30 0.25 0.04 0.02-0.10 0.02-0.07
    AWS RULES 0.08-0.13 1.20 0.30 8-10.5 0.85-1.2 0.80 0.01 0.01 0.15-0.30 0.25 0.04 0.02-0.10 0.02-0.07
    EXAMPLE VALUE 0.092 0.7 0.24 9 9 0.48 0.008 0.006 0.2 0.02 0.001 0.04 0.03

     

    MECHANICAL PROPERTY:

    PROPERTY YIELD STRENGTH(MPa) EXTENSION STRENGTH(MPa) IMAPACT VALUE J/℃ ELONGATION(%) Heat treatment°Cxh
    GB/T RULES 530 620 - 15 760*2
    AWS RULES 530 620 - 17 760*2
    EXAMPLE VALUE 585 730 78/Normal temperature 20 760*2

     

    RECOMMENDED WELDING PARAMETERS:

    DIAMETERS SPECIFICATIONS(mm) 2.6*350 3.2*350 4.0*400 5.0*400
    ELECTRICITY
    (Amp)
    H/W 80-110 100-130 130-180 170-210
    O/W 60-100 80-120 120-160 -