Low-alloy steels Manual electrode E9018-B3 Seal accessories
Low hydrogen potassium type hand electrode, under 550C high temperature working conditions still has excellent creep resistance
Stable arc, less splash, good molding, easy slag removal, X-Ray performance
Under special heat treatment conditions, stable low temperature impact performance can still be guaranteed
CHEMICAL COMPONET:
ALLOY(wt%) | C | Si | Mn | P | S | Ni | Cr | Mo | Other |
GB/T RULES | 0.07 | 0.35 | 0.75 | 0.011 | 0.013 | 0.02 | 2.28 | 1.05 | - |
MECHANICAL PROPERTY:
PROPERTY | YIELD STRENGTH(MPa) | EXTENSION STRENGTH(MPa) | Elongation(%) | IMAPACT VALUE J/℃ | Heat treatment °C*h | |||||
GB/T RULES | 575 | 675 | 19.5 | 160/Normal temperature | 690*1 |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 3.2*350 | 4.0*400 | 5.0*400 | ||||
ELECTRICITY (Amp) |
H/W | 90-130 | 140-190 | 190-240 | |||
O/W | 80-120 | 120-160 | - |
Reactor internals
8.2 ton bulk carrier
-
Qinghai Youjian Wunan oilfield
CHEMICAL COMPONET:
ALLOY(wt%) | C | Si | Mn | P | S | Ni | Cr | Mo | Other |
GB/T RULES | 0.07 | 0.35 | 0.75 | 0.011 | 0.013 | 0.02 | 2.28 | 1.05 | - |
MECHANICAL PROPERTY:
PROPERTY | YIELD STRENGTH(MPa) | EXTENSION STRENGTH(MPa) | Elongation(%) | IMAPACT VALUE J/℃ | Heat treatment °C*h | |||||
GB/T RULES | 575 | 675 | 19.5 | 160/Normal temperature | 690*1 |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 3.2*350 | 4.0*400 | 5.0*400 | ||||
ELECTRICITY (Amp) |
H/W | 90-130 | 140-190 | 190-240 | |||
O/W | 80-120 | 120-160 | - |