Low-alloy steels X70 line steel E81T5-GC weld fabrication stuff
CHEMICAL COMPONET:
ALLOY(wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | Al |
GB/T RULES | 0.15 | 0.5-1.75 | 0.80 | - | 1.00-2.00 | 0.35 | 0.03 | 0.03 | - |
AWS RULES | - | - | - | - | - | - | - | - | - |
EXAMPLE VALUE | 0.065 | 1.00 | 0.1 | 0.01 | 1.8 | 0.01 | 0.01 | 0.002 | 1.00 |
MECHANICAL PROPERTY:
PROPERTY | YIELD STRENGTH(MPa) | EXTENSION STRENGTH(MPa) | IMAPACT VALUE J/℃ | ELONGATION(%) | Heat treatment°Cxh | |||||
GB/T RULES | 460 | 550-740 | 27/-40 | 17 | AW | |||||
AWS RULES | 460 | 550-690 | - | 19 | AW | |||||
EXAMPLE VALUE | 510 | 585 | 150/-40 | 25 | AW |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 1.2/ Automatic welding | 1.4/ Automatic welding | 1.6/ Semi-automatic welding | |||||||
Fill | Capping | Fill | Capping | |||||||
Volt | 23-25 | 20-22 | 24-27 | 22-24 | 21-24 | |||||
Amp | 220-260 | 180-200 | 240-300 | 190-220 | 200-250 | |||||
Dry extension length(mm) | 15-20 | 15-20 | 15-20 | 15-20 | 15-20 | |||||
Gas flow(l/min) | 15-25 | 15-25 | 15-25 | 15-25 | 15-25 |
Flux-cored welding wire, 550Mpa alkaline low-alloy steel.
Beautiful forming, good slag removal, less smoke, with excellent welding technology, suitable for vertical downward welding.
It has good low temperature toughness, crack resistance and porosity resistance.
-
Harbin Electric - Sanmen, Haiyang MSR
-
Carbon steel, stainless steel tower welding
-
2.3 million barrels of SBM Fast4ward FPSO
CHEMICAL COMPONET:
ALLOY(wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | Al |
GB/T RULES | 0.15 | 0.5-1.75 | 0.80 | - | 1.00-2.00 | 0.35 | 0.03 | 0.03 | - |
AWS RULES | - | - | - | - | - | - | - | - | - |
EXAMPLE VALUE | 0.065 | 1.00 | 0.1 | 0.01 | 1.8 | 0.01 | 0.01 | 0.002 | 1.00 |
MECHANICAL PROPERTY:
PROPERTY | YIELD STRENGTH(MPa) | EXTENSION STRENGTH(MPa) | IMAPACT VALUE J/℃ | ELONGATION(%) | Heat treatment°Cxh | |||||
GB/T RULES | 460 | 550-740 | 27/-40 | 17 | AW | |||||
AWS RULES | 460 | 550-690 | - | 19 | AW | |||||
EXAMPLE VALUE | 510 | 585 | 150/-40 | 25 | AW |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 1.2/ Automatic welding | 1.4/ Automatic welding | 1.6/ Semi-automatic welding | |||||||
Fill | Capping | Fill | Capping | |||||||
Volt | 23-25 | 20-22 | 24-27 | 22-24 | 21-24 | |||||
Amp | 220-260 | 180-200 | 240-300 | 190-220 | 200-250 | |||||
Dry extension length(mm) | 15-20 | 15-20 | 15-20 | 15-20 | 15-20 | |||||
Gas flow(l/min) | 15-25 | 15-25 | 15-25 | 15-25 | 15-25 |