Stainless steels Flux cored wire E2553T1-1 metal Jointing accessories

GB/T17853 TS 2553-F C1 1

AWS A5.22 E2253T1-1

A5.22M E2253T1-1

ISO 17633-B:TS 2253-F C1 1

Whatapp:+8613252436578

E-mail: sale@welding-honest.com


  • Brand: JINGLEI
  • Model: GFS-2553
  • Power supply polarity: DC+
  • Origin: China
  • Suit for: Stainless steels
  • Size: 1.2mm 1.6mm
  • MOQ:1T Capacity: 6000T Per month
  • Payment: TT,LC
  • OEM: Can customerized
  • Product Detail

    SPECIFICATION

    Product Tags

    未标题-1
    57744501231
    1e80a01238

    Application

    Suitable for welding of dual phase steel containing 25% Cr stainless steel, such as 00 cr25ni7mo4n, 03 cr25ni6mo3cu2n, UNS 32550 (Alloy255), etc.

    CHEMICAL COMPONET:

    ALLOY(wt%) C Mn Si Cr Ni Mo P S Else
    GB/T RULES 0.04 0.5-1.5 0.75 24.0-27.0 8.5-10.5 2.9-3.9 0.04 0.03 Cu:1.5-2.5/N:0.10-0.25
    AWS RULES 0.04 0.5-1.5 0.75 24.0-27.0 8.5-10.5 2.9-3.9 0.04 0.03 Cu:1.5-2.5/N:0.10-0.25
    EXAMPLE VALUE 0.023 0.65 0.6 25 9 3.5 0.015 0.002 Cu:1.70/N:0.12

     

    MECHANICAL PROPERTY:

    PROPERTY YIELD STRENGTH(MPa) EXTENSION STRENGTH(MPa) IMAPACT VALUE J/℃ ELONGATION(%)
    GB/T RULES - 760 - 13
    AWS RULES - 760 - 15
    EXAMPLE VALUE - 840 - 25

     

    RECOMMENDED WELDING PARAMETERS:

    DIAMETERS SPECIFICATIONS(mm) 1.2 1.6
    Volt 22-36 26-38
    Amp 120-260 200-300
    Dry extension length(mm) 15-20 18-25
    Gas flow(l/min) 15-25 15-25

    Peculiarity

    03

    The main components are low 25.5%Cr-9.5%Ni-3.4%Mo-2%Cu-0.18%N;

    The weld metal is austenitic ferrite biphase structure with high strength and good resistance to pitting and stress corrosion cracking.

    02
    01

    The arc is soft and stable, less splash, beautiful forming, good slag removal, stable wire feeding, with excellent welding process performance.

    Show details

    04
    05

    Soft and stable arc

    Less splash

    About us

    A4

    Factory fioor display

    33
    34
    35
    36

    Application case

    01
    02

    Zhejiang Petrochemical 40 million tons/year refining and chemical integration project

    Welding materials for aluminum alloys

    Actual factory shooting

    577445SDA01

    CHEMICAL COMPONET:

    ALLOY(wt%) C Mn Si Cr Ni Mo P S Else
    GB/T RULES 0.04 0.5-1.5 0.75 24.0-27.0 8.5-10.5 2.9-3.9 0.04 0.03 Cu:1.5-2.5/N:0.10-0.25
    AWS RULES 0.04 0.5-1.5 0.75 24.0-27.0 8.5-10.5 2.9-3.9 0.04 0.03 Cu:1.5-2.5/N:0.10-0.25
    EXAMPLE VALUE 0.023 0.65 0.6 25 9 3.5 0.015 0.002 Cu:1.70/N:0.12

     

    MECHANICAL PROPERTY:

    PROPERTY YIELD STRENGTH(MPa) EXTENSION STRENGTH(MPa) IMAPACT VALUE J/℃ ELONGATION(%)
    GB/T RULES - 760 - 13
    AWS RULES - 760 - 15
    EXAMPLE VALUE - 840 - 25

     

    RECOMMENDED WELDING PARAMETERS:

    DIAMETERS SPECIFICATIONS(mm) 1.2 1.6
    Volt 22-36 26-38
    Amp 120-260 200-300
    Dry extension length(mm) 15-20 18-25
    Gas flow(l/min) 15-25 15-25