Stainless steels Manual electrode E2594-16 Soldering makings
Application
It is suitable for welding of 25%Cr duplex stainless steel in offshore oil, natural gas and petrochemical industries. For example, 0022CrNi7Mo4N, 03Cr25Ni6Mo3Cu2N, UNS 32550 (Alloy255) UNS S32750.
Certification body:BV、CCS、LR、NK
CHEMICAL COMPONET:
ALLOY(wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | N | Cu | |
GB/T RULES | 0.04 | 0.5-2.0 | 1.00 | 24.0-27.0 | 8.0-10.5 | 3.4-4.5 | 0.04 | 0.03 | 0.20-0.30 | 0.75 | |
AWS RULES | 0.04 | 0.5-2.0 | 1.00 | 24.0-27.0 | 8.0-10.5 | 3.4-4.5 | 0.04 | 0.03 | 0.20-0.30 | 0.75 | |
EXAMPLE VALUE | 0.021 | 0.85 | 0.74 | 25.2 | 9.1 | 4.05 | 0.021 | 0.005 | 0.25 | 0.05 |
MECHANICAL PROPERTY:
PROPERTY | YIELD STRENGTH(MPa) | EXTENSION STRENGTH(MPa) | IMAPACT VALUE J/℃ | ELONGATION(%) | ||||
GB/T RULES | - | 760 | - | 13 | ||||
AWS RULES | - | 760 | - | 15 | ||||
EXAMPLE VALUE | - | 915 | - | 22.5 |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 2.0*250 | 2.6*300 | 3.2*350 | 4.0*350 | 5.0*350 | |||||
ELECTRICITY (Amp) |
H/W | 50-75 | 70-95 | 80-120 | 110-160 | 160-190 | ||||
O/W | 20-50 | 45-80 | 70-110 | 90-135 | - |
Titanium-calcium two-phase stainless steel hand electrode, the main component is 25.5Cr-10Ni-4Mo-0.25N;
Weld metal is austenitic ferrite biphase structure, with high strength, good pitting and stress corrosion cracking resistance, excellent thermal crack resistance, PREN (pitting resistance equivalent) ≥40.
Ningbo Honest Metal Materials Co,Ltd.is an international welding professional company withindependent research and development, production, sales and management. It was established in 2020.
85000 m3 Very Large ethane Ethylene Carrier (VLEC)
Harbin Electric - Sanmen, Haiyang MSR
Polypropylene reactor
CHEMICAL COMPONET:
ALLOY(wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | N | Cu | |
GB/T RULES | 0.04 | 0.5-2.0 | 1.00 | 24.0-27.0 | 8.0-10.5 | 3.4-4.5 | 0.04 | 0.03 | 0.20-0.30 | 0.75 | |
AWS RULES | 0.04 | 0.5-2.0 | 1.00 | 24.0-27.0 | 8.0-10.5 | 3.4-4.5 | 0.04 | 0.03 | 0.20-0.30 | 0.75 | |
EXAMPLE VALUE | 0.021 | 0.85 | 0.74 | 25.2 | 9.1 | 4.05 | 0.021 | 0.005 | 0.25 | 0.05 |
MECHANICAL PROPERTY:
PROPERTY | YIELD STRENGTH(MPa) | EXTENSION STRENGTH(MPa) | IMAPACT VALUE J/℃ | ELONGATION(%) | ||||
GB/T RULES | - | 760 | - | 13 | ||||
AWS RULES | - | 760 | - | 15 | ||||
EXAMPLE VALUE | - | 915 | - | 22.5 |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 2.0*250 | 2.6*300 | 3.2*350 | 4.0*350 | 5.0*350 | |||||
ELECTRICITY (Amp) |
H/W | 50-75 | 70-95 | 80-120 | 110-160 | 160-190 | ||||
O/W | 20-50 | 45-80 | 70-110 | 90-135 | - |