Stainless steels Manual electrode E347L-16 weld fabrication data
Application
It is suitable for welding 18%Cr-8%Ni-Nb stainless steel (SUS347) and 18%Cr-8%Ni-Ti stainless steel (sus321) in petrochemical industry, pressure vessel, food machinery, medical machinery, chemical fertilizer and other industries.
CHEMICAL COMPONET:
ALLOY(wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | else | |
GB/T RULES | 0.04 | 0.5-2.5 | 1.00 | 18.0-21.0 | 9.0-11.0 | 0.75 | 0.04 | 0.03 | Cu0.75/Nb:8C-1.00 | |
AWS RULES | 0.08 | 0.5-2.5 | 1.00 | 18.0-21.0 | 9.0-11.0 | 0.75 | 0.04 | 0.03 | Cu0.75/Nb:8C-1.00 | |
EXAMPLE VALUE | 0.033 | 0.84 | 0.69 | 18.7 | 9.5 | 0.1 | 0.027 | 0.005 | Cu0.22/Nb0.50 |
MECHANICAL PROPERTY:
PROPERTY | YIELD STRENGTH(MPa) | EXTENSION STRENGTH(MPa) | IMAPACT VALUE J/℃ | ELONGATION(%) | ||||
GB/T RULES | - | 510 | - | 25 | ||||
AWS RULES | - | 520 | - | 30 | ||||
EXAMPLE VALUE | - | 615 | - | 36 |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 2.0*250 | 2.6*300 | 3.2*350 | 4.0*350 | 5.0*350 | |||||
ELECTRICITY (Amp) |
H/W | 50-75 | 70-95 | 80-120 | 110-160 | 160-190 | ||||
O/W | 20-50 | 45-80 | 70-110 | 90-135 | - |
Titanium calcium stainless steel hand electrode, the main composition is low carbon 18%Cr-9%Ni-Nb;When Nb is added on the basis of 308, the carbon content is lower at the same time, which can effectively improve the corrosion resistance, especially the intergranular corrosion performance.
Stable arc, beautiful forming, delicate ripple, little splash, easy slag removal, good fire resistance, good porosity resistance.
Ningbo Honest Metal Materials Co,Ltd.is an international welding professional company withindependent research and development, production, sales and management. It was established in 2020.
Xinjiang Kela 2 central processing plant project
Welding materials for containers
Gansu Lanke Petrochemical -50℃ propane spherical tank project
CHEMICAL COMPONET:
ALLOY(wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | else | |
GB/T RULES | 0.04 | 0.5-2.5 | 1.00 | 18.0-21.0 | 9.0-11.0 | 0.75 | 0.04 | 0.03 | Cu0.75/Nb:8C-1.00 | |
AWS RULES | 0.08 | 0.5-2.5 | 1.00 | 18.0-21.0 | 9.0-11.0 | 0.75 | 0.04 | 0.03 | Cu0.75/Nb:8C-1.00 | |
EXAMPLE VALUE | 0.033 | 0.84 | 0.69 | 18.7 | 9.5 | 0.1 | 0.027 | 0.005 | Cu0.22/Nb0.50 |
MECHANICAL PROPERTY:
PROPERTY | YIELD STRENGTH(MPa) | EXTENSION STRENGTH(MPa) | IMAPACT VALUE J/℃ | ELONGATION(%) | ||||
GB/T RULES | - | 510 | - | 25 | ||||
AWS RULES | - | 520 | - | 30 | ||||
EXAMPLE VALUE | - | 615 | - | 36 |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 2.0*250 | 2.6*300 | 3.2*350 | 4.0*350 | 5.0*350 | |||||
ELECTRICITY (Amp) |
H/W | 50-75 | 70-95 | 80-120 | 110-160 | 160-190 | ||||
O/W | 20-50 | 45-80 | 70-110 | 90-135 | - |