Stainless steels SAW welding wire ER308 and flux Welding materials
WELDING TECHNOLOGY
Don't let the questions
Continue to haunt you
Arc instability
Unsightly molding
Excessive spatter
Widely used in petrochemical, pressure vessels, food machinery
Medical equipment and other related industries.
Ripple fine
18%Cr-8%Ni stainless steel welding (SUS304)
Good weldability, crack resistance sensitivity.
Easy slagging
Product Parameter
CHEMICAL COMPONET:
ALLOY(wt%) | C | Si | Mn | P | S | Ni | Cr | Mo |
GB/T RULES | 0.025 | 0.65 | 1.5 | 0.025 | 0.002 | 9.7 | 20.2 | - |
MECHANICAL PROPERTY:
PROPERTY | Strength of extension(Mpa) | Elongation/% | IMAPACT VALUE J/℃ | Intergranular corrosion | ||||
GB/T RULES | 580 | 38 | ≥31/-196 | GB/T4334E method passed |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 2.4 | 3.2 | 4.0 | ||||
Volt | 28-32 | 28-32 | 28-32 | ||||
Amp | 270-360 | 400-550 | 500-650 | ||||
Velocity(mm/min) | 250-320 | 300-420 | 400-480 | ||||
Dry elongation(mm) | 20-24 | 22-26 | 30-34 |
Factory support
The product is suitable for a
wide range of applications
WELDING TECHNOLOGY
JU2000E jack-up
drilling platform
-
49,000 tons of duplex
stainless steel chemical tanker
-
Zhejiang Satellite Energy
3× 60,000 m³LPG storage tank
CHEMICAL COMPONET:
ALLOY(wt%) | C | Si | Mn | P | S | Ni | Cr | Mo |
GB/T RULES | 0.025 | 0.65 | 1.5 | 0.025 | 0.002 | 9.7 | 20.2 | - |
MECHANICAL PROPERTY:
PROPERTY | Strength of extension(Mpa) | Elongation/% | IMAPACT VALUE J/℃ | Intergranular corrosion | ||||
GB/T RULES | 580 | 38 | ≥31/-196 | GB/T4334E method passed |
RECOMMENDED WELDING PARAMETERS:
DIAMETERS SPECIFICATIONS(mm) | 2.4 | 3.2 | 4.0 | ||||
Volt | 28-32 | 28-32 | 28-32 | ||||
Amp | 270-360 | 400-550 | 500-650 | ||||
Velocity(mm/min) | 250-320 | 300-420 | 400-480 | ||||
Dry elongation(mm) | 20-24 | 22-26 | 30-34 |